Journal of Liaoning Petrochemical University

Journal of Liaoning Petrochemical University ›› 2017, Vol. 37 ›› Issue (2): 48-53.DOI: 10.3969/j.issn.1672-6952.2017.02.011

Previous Articles     Next Articles

Three Reminders Pressure Inlet Filter Short Cracking Failure Analysis

Fu Liang,Zhang Guofu,Liu Dan   

  1. Schoolof Mechanical Engineering,Liaoning Shihua University,Fushun Liaoning 113001,China
  • Received:2016-05-25 Revised:2016-08-25 Published:2017-04-20 Online:2017-05-04

三催气压机入口过滤器短接开裂失效原因分析

付 亮,张国福,刘 丹   

  1. 辽宁石油化工大学机械工程学院,辽宁 抚顺 113001
  • 通讯作者: 张国福(1960-),男,硕士,教授,从事金属材料性能研究;E-mail:zgf-fs@163.com
  • 作者简介:作者简介:付亮(1983-),男,硕士研究生,从事压力容器与结构完整性技术方面的研究;E-mail:289494984@qq.com

Abstract:       Pressure machine inlet filter short piping could produce cracks in a short time. Crack parts of the macroscopic examination, chemical composition analysis, tissue imaging, scanning electron microscopy analysis, and mechanical analysis were studied. The results showed that in the corrosive medium containing H2S, the flange and the nozzle were subjected to welding residual stress during the manufacturing process, and the welding residual stress caused stress corrosion, resulting in cracking along the embrittlement.

Key words: Pressure machine,    , Stress corrosion,    , Welding,    , Crack,    , Mechanical properties

摘要:         三催气压机入口过滤器短接在很短的时间内会产生裂纹。对裂纹部位进行了宏观检验、化学成分分析、显像组织分析、扫描电镜分析、力学性能分析。分析结果得知,裂纹产生的主要原因如下:工件在含有H2S的腐蚀介质中,法兰与接管在加工制造过程中产生焊接残余应力,在腐蚀介质与残余应力的共同作用下导致应力腐蚀,从而产生沿晶脆性开裂。针对断裂原因提出了改进方案。

关键词: 气压机,    ,  焊缝,   ,  应力腐蚀,   ,  裂纹,    , 力学性能

Cite this article

Fu Liang,Zhang Guofu,Liu Dan. Three Reminders Pressure Inlet Filter Short Cracking Failure Analysis[J]. Journal of Liaoning Petrochemical University, 2017, 37(2): 48-53.

付 亮,张国福,刘 丹. 三催气压机入口过滤器短接开裂失效原因分析[J]. 辽宁石油化工大学学报, 2017, 37(2): 48-53.